Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.208 J/cm | 0.390 ft-lb/in | ASTM D256 |
Plenco 7200 Phenolic, Granular, Injection Molded PLENCO 07200 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength, good powder properties and excellent cosmetic properties. UL recognized under component .. |