Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | >= 19.0 J/cm² | >= 90.4 ft-lb/in² | Determined with double-notched specimens; ISO 11542-2 |
Braskem UTEC® 3040 Ultra High Molecular Weight Polyethylene Description: UTEC3040 is an Ultra High Molecular Weight Polyethylene with a molecular weight about 10 times higher than High Density Polyethylene (HDPE) resins. This extremely high molecular weight .. |
|||
Charpy Impact, Notched | 19.0 J/cm² @Temperature -20.0 °C |
90.4 ft-lb/in² @Temperature -4.00 °F |
After conditioning at 23°C/50%RH; ISO 179/Af |
Arkema Group Orgalloy® RS 6030 Polyamide 6 Alloy 30% Glass Fiber reinforced Polyamide Alloy, Rigid grade, Nylon 6 basedMolding of Engineering PartsInformation provided by Arkema Group |