Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.64 J/cm² @Temperature 23.0 °C |
7.80 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1A |
Gromax BFG30-B103N1 Nylon 6 33% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |