Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.57 J/cm²

@Temperature 22.8 °C
7.50 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
Polymer Resources PPX-FR5 Modified-PPO, V-0 Flame Retardant
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 225F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
Charpy Impact, Notched 1.57 J/cm²

@Temperature 22.8 °C
7.50 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
Polymer Resources PPX-GP4 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 210F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..