Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.56 J/cm²
7.42 ft-lb/in²
EN ISO 179/1eA
Wolf Kunststoff ZEDEX® ZX-750V5KF 055 Polymer Alloy. Fiber Reinforced
Main Characteristics: Stiff; High elongation and yield stress; Low thermal expansion; Impact resistantApplications: Textile Machinery; Compressors; Hinges; Handling; Machine Tools; Automitve Technol..
Copyright © lookpolymers.com All Rights Reserved