Mechanical Properties Metric English Comments
Charpy Impact, Notched 12.9 J/cm²

@Temperature 23.0 °C
61.4 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Xenoy® EXXY0113 PBT (Asia Pacific)
Blow Moldable Impact modified XENOYThis data was supplied by SABIC-IP for the Asia Pacific region.
Charpy Impact, Notched 12.9 J/cm²

@Temperature 23.0 °C
61.4 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Xenoy® EXXY0113 PBT (Europe-Africa-Middle East)
Blow Moldable Impact modified XENOYThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Charpy Impact, Notched 12.9 J/cm²

@Temperature 23.0 °C
61.4 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Xenoy® X6800BM PBT
Blow moldable, impact modifed XENOYThis data was supplied by SABIC-IP for the Americas region.
Charpy Impact, Notched 12.9 J/cm²
61.4 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Xenoy® X6800BM PBT (Asia Pacific)
Blow moldable, impact modifed XENOY
Charpy Impact, Notched 12.9 J/cm²
61.4 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Xenoy® X6800BM PBT (Europe-Africa-Middle East)
Blow moldable, impact modifed XENOY