Mechanical Properties Metric English Comments
Charpy Impact, Notched 60.0 J/cm²
286 ft-lb/in²
J/m; ASTM D256
PolyOne Edgetek® XP9242701 Polyphenylene Sulfide (PPS)
Injection Speed: 50 to 80% Holding Time: 3 to 9 sec Injection Time: 1 to 3 sec Cycle Time: 18 to 70 secInformation provided by PolyOne
Charpy Impact, Notched 60.0 - 100 J/cm²
286 - 476 ft-lb/in²
Plansee DENAL® 910 179 20 Tungsten-Nickel-Iron-Cobalt Alloy
Characteristics:exceptionally stronghigh densityoutstanding mechanical damping capabilitiesHigh absorption of X-ray and gamma radiationInformation provided by Plansee.
Charpy Impact, Notched 60.0 - 100 J/cm²
286 - 476 ft-lb/in²
Plansee DENAL® 920 60 20 Tungsten-Nickel-Iron-Cobalt Alloy
Characteristics:exceptionally stronghigh densityoutstanding mechanical damping capabilitiesHigh absorption of X-ray and gamma radiationInformation provided by Plansee.