Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 11.8 J/cm²
56.2 ft-lb/in²
Arkema Group Kynar® FLEX 2750 PVDF  (discontinued **)
Designation ISO 12086-VDF/HFP-K, EG1NS, M. ?E7.B.F.A.C,, ? (4-10)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, imperviousne..