Polymer Property : Charpy Impact, Notched = 5.81 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.22 J/cm²
5.81 ft-lb/in²
Arkema Group Rilsan® BZM 43 G9 Nylon 11, 43% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA11,MS,18-080,(G+C)(F+D)(45+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Additive free.High rigidity. Hig..
Charpy Impact, Notched 1.22 J/cm²

@Temperature -30.0 °C
5.81 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® 8020 Nylon 11, Flexible Tubing Grade (Conditioned)
Designation ISO 1874-PA11/xx,E,16-003Transparent and flexible copolymer for tubes extrusion. Additive free.Good flexibility. Very good transparency. High chemical resistance.USP XXIII class VI appro..