Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 100 - 150 J/cm² | 476 - 714 ft-lb/in² | |
Plansee DENAL® 920 159 20 Tungsten-Nickel-Iron-Cobalt Alloy Characteristics:exceptionally stronghigh densityoutstanding mechanical damping capabilitiesHigh absorption of X-ray and gamma radiationInformation provided by Plansee. |