Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 47.59 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 10.00 J/cm²

@Temperature -30.0 °C
47.59 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
BASF Ultramid® A3X2G7 35% Glass Filled PA66 (Dry)
Ultramid A3X2G7 is a 35% glass fiber reinforced injection molding PA66 grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; very high stif..