Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 8.40 J/cm² | 40.0 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® C 216 PA6, Conditioned Description: Unreinforced polyamide PA6, standard nucleation for fast cycling, for injection molding.Available in: Asia PacificProduct Applications: This grade has a high fluidity and good mould rel.. |