Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 4.40 J/cm² | 20.9 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 HS28 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, maximum cold and dry impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 4.40 J/cm² @Temperature -30.0 °C |
20.9 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® EXCY0025 PC+ABS Recyle Material with PC+ABS+EXL recycle for good low temperature impact performance. |
|||
Charpy Impact, Notched | 4.40 J/cm² | 20.9 ft-lb/in² | ISO Data |
Styron Magnum™ HPC 952 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |