Polymer Property : Charpy Impact, Notched = 31.0 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.231 - 6.51 J/cm²
1.10 - 31.0 ft-lb/in²
Average value: 1.42 J/cm² Grade Count:38
Overview of materials for Ethylene Butyl Acrylate
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Butyl Acrylate". Each property range of values reported is minimum and maximum values of approp..