Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.670 J/cm² | 3.19 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL A63 FK 2010 Nylon 6.6 for injection molding, 20% glass fiber and 10% glass ball reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.670 J/cm² | 3.19 ft-lb/in² | ISO 179/1eA |
Radici Radilon® ALX14080 (dry) Nylon 66 Medium high viscosityInformation provided by Radici group. |
|||
Charpy Impact, Notched | 0.670 J/cm² | 3.19 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 60 G1 V30 PA66, 30% glass fiber, DRY Description: Flame retardant Polyamide PA66 reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This R.. |
|||
Charpy Impact, Notched | 0.670 J/cm² | 3.19 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® 3200 Polybutylene Terephthalate (PBT), Standard, 20% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 0.670 J/cm² | 3.19 ft-lb/in² | |
Eastman Eastar 6763 PETG Copolyester ISO data as provided by the manufacturer, Eastman Chemical |
|||
Charpy Impact, Notched | 0.670 J/cm² | 3.19 ft-lb/in² | |
Arkema Group Rilsan® ARVO 950 TLD Nylon 12, Rotomolding Grade (Conditioned) Designation ISO 1874-PA12,RHLR,16-010Grade for rotomolding. Available color: natural. Light and heat stabilized. Mold-release agent.Easy to be processed in the same conditions as polyethylene. High .. |