Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 5.50 J/cm² | 26.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS (Asia Pacific) CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only. |
|||
Charpy Impact, Notched | 5.50 J/cm² | 26.2 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS (Asia Pacific) High impact PC+ABS material designed for local Pacific Automotive applications |
|||
Charpy Impact, Notched | 5.50 J/cm² | 26.2 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Charpy Impact, Notched | 5.50 J/cm² | 26.2 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Charpy Impact, Notched | 5.50 J/cm² | 26.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul.. |
|||
Charpy Impact, Notched | 5.50 J/cm² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HPX4 PC Copolymer Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP.. |
|||
Charpy Impact, Notched | 5.50 J/cm² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® ML3400 PC (Europe-Africa-Middle East) LEXAN ML3400 is a medium viscosity, impact modified grade with improved chemical resistance. It passes the British Standard 2495 and 5361 solvent tests. |
|||
Charpy Impact, Notched | 5.50 J/cm² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1A |
Gromax BPR20-N1 Nylon 6, Flame Retardant (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact, Notched | 5.50 J/cm² | 26.2 ft-lb/in² | ISO 179/1EA-1993 |
Solvay Technyl® A 246M Nylon 66, Impact Grade, EH0 Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Technyl A 246m offers an excellent notched impact resistance at low temperatures makin.. |
|||
Charpy Impact, Notched | 5.50 J/cm² | 26.2 ft-lb/in² | 80*10*4mm, Cut; ISO 179/1eA |
SABIC Innovative Plastics SABIC PPCOMPOUND 8620A PP SABIC® PPcompound 8620A is a mineral filled, impact modified polypropylene TPO. It was originally designed for painted automotive bumper fascia applications where a combination of good flow, hig.. |
|||
Charpy Impact, Notched | 5.50 J/cm² | 26.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance. |
|||
Charpy Impact, Notched | 5.50 J/cm² | 26.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC (Asia Pacific) Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance. |
|||
Charpy Impact, Notched | 5.50 J/cm² | 26.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Asia Pacific) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Charpy Impact, Notched | 5.50 J/cm² | 26.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Charpy Impact, Notched | 5.50 J/cm² | 26.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty.. |
|||
Charpy Impact, Notched | 5.50 J/cm² | 26.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC (Asia Pacific) Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty.. |
|||
Charpy Impact, Notched | 5.50 J/cm² | 26.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC (Europe-Africa-Middle East) Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im.. |
|||
Charpy Impact, Notched | 5.50 J/cm² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Styrolution Terblend® N NM-13 ABS/PA6 (Dry) Terblend N NM-13 is a new experimental ABS/PA6-Blend with improved impact strength at low temperatures. It can be easily processed on any standard injection molding machine.Information provided by .. |
|||
Charpy Impact, Notched | 5.50 J/cm² | 26.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Asia Pacific) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Charpy Impact, Notched | 5.50 J/cm² | 26.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Europe-Africa-Middle East) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Charpy Impact, Notched | 5.50 J/cm² | 26.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® XD1588 PBT+PC (Europe-Africa-Middle East) PBT+PC blend for painted automotive exterior applications, having good flow. |
|||
Charpy Impact, Notched | 5.50 J/cm² | 26.2 ft-lb/in² | ISO 179/1eA |
Styron CALIBREâ„¢ 300-6 Polycarbonate Resin Overview: CALIBREâ„¢ 300-6 polycarbonate resin offer exceptional impact resistance, heat distortion resistance, and optical clarity as high melt strength for blow molding and sheet applications. .. |
|||
Charpy Impact, Notched | 5.50 J/cm² | 26.2 ft-lb/in² | ISO 179/1eA |
Covestro Makroblend® DP 7645 Polycarbonate + PET, Impact Grade Developmental productISO 7792-PC/PET,MHPR,-020(PC/PET)-blends, impact modifiedInjection molding gradeunreinforcedPreprocessingMax. Water content |
|||
Charpy Impact, Notched | 5.50 J/cm² | 26.2 ft-lb/in² | ISO 179/1eA |
Covestro Makroblend® DP UT3907 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendhigh flowimpact modifiedeasy releaseUV-stabilizedinjection molding grade Makroblend DP UT3907* offers superior flowability, good impact strength and excellent ch.. |
|||
Charpy Impact, Notched | 5.50 J/cm² | 26.2 ft-lb/in² | ISO 179/1eA |
Covestro Makroblend® DP UT5005 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendimpact modifiedeasy releaseinjection molding gradeMakroblend DP UT5005* provides an outstanding balance of low-temperature impact strength and flowability beside e.. |
|||
Charpy Impact, Notched | 5.50 J/cm² | 26.2 ft-lb/in² | ISO 179/1eA |
Covestro Makroblend® DP UT5007 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendimpact modifiedeasy releaseUV-stabilizedinjection molding grade Makroblend DP UT5007* provides an outstanding balance of low-temperature impact strength and flow.. |
|||
Charpy Impact, Notched | 5.50 J/cm² | 26.2 ft-lb/in² | |
Arkema Group Rilsan® MB 3501 Nylon 11, Flexible Tubing Grade (Dry) Designation ISO 1874-PA11-HI,MHL,22-004Flexible grade for tubes extrusion. Available color: black. Light and heat stabilized.Flexibility. High burst pressure and impact strength. Fit for use in a wi.. |
|||
Charpy Impact, Notched | 5.50 J/cm² | 26.2 ft-lb/in² | |
BASF Novolen® 2700 L Polypropylene UV stabilized grade for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 5.50 J/cm² | 26.2 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |