Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 25.7 J/cm² | 122 ft-lb/in² | ISO 179 |
Menzolit Menzolit® HPC 1200 Unsaturated Polyester UP HPC 1200 is a special SMC for high strength applications. The glass level has been selected to combine mouldability with high strength and stiffness properties in orientation direction. The reinforc.. |