Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.490 - 2.42 J/cm² @Temperature -30.0 - -30.0 °C |
2.33 - 11.5 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 1.17 J/cm² Grade Count:18 |
Overview of materials for Nylon 11, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |