Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.472 J/cm² | 2.25 ft-lb/in² | ISO 179-1:2007 |
CRP Technology Windform® GF 2.0 Polyamide-Aluminum-Glass Composite Processed by selective laser sintering (SLS). Windform® GF 2.0 is the evolutionary substitute for Windform GF, our first generation material. Windform® GF 2.0 is a composite material made of poly.. |
|||
Charpy Impact, Notched | 0.472 J/cm² | 2.25 ft-lb/in² | ISO 179-1:2007 |
CRP Technology Windform® XT 2.0 Polyamide-Carbon Fiber Composite Processed by selective laser sintering (SLS). Windform® XT 2.0 is the evolution of the ground breaking high performance Windform® XT, the carbon fiber reinforced composite material, known for its.. |
|||
Charpy Impact, Notched | 0.473 J/cm² | 2.25 ft-lb/in² | ASTM D256 and UNI EN ISO 179:1998 |
CRP Technology Windform® XT Polyamide-Carbon Composite WindForm™ XT Composite is a new generation material, in which the mechanical characteristics are excellent for Rapid Manufacturing. Black coloured compound polyamide and carbon based material with .. |