Mechanical Properties Metric English Comments
Charpy Impact, Notched 2.25 J/cm²
10.7 ft-lb/in²
After conditioning at 23°C/50%RH; ISO 179/Af
Arkema Group Orgalloy® RS 6635 A Polyamide 6.6 Alloy 35% Glass Fiber reinforced
Polyamide Alloy, Rigid grade, Nylon 6.6 basedMolding of Engineering PartsInformation provided by Arkema Group