Polymer Property : Charpy Impact, Notched = 19.5 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 4.10 J/cm²
19.5 ft-lb/in²
Ineos ABS Lustran® 752
Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Sheet extrusionThermoforming
Charpy Impact, Notched 4.10 J/cm²
19.5 ft-lb/in²
ISO 179-1
Unitika A1030BRL PA6, Conditioned
Information provided by Unitika Ltd.
Charpy Impact, Notched 4.10 J/cm²
19.5 ft-lb/in²
ISO 179-1
Unitika A1030SR PA6, Conditioned
Information provided by Unitika Ltd.