Mechanical Properties Metric English Comments
Charpy Impact, Notched 3.67 J/cm²
17.5 ft-lb/in²
Arkema Group Rilsan® BMN P20 D Nylon 11 (Conditioned)
Designation ISO 1874-PA11-P,MR,12-004Flexible grade for injection molding. Available colors: black and natural. Mold release agent.Outstanding working properties. Easy filling of the mold due to its..