Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 3.24 J/cm² | 15.4 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® C 218 V33 PA6, 33% glass fiber, Eh 50 Description: Polyamide PA6, reinforced with 33% of glass fiber, heat stabilized, for injection molding.Applications: It has good mechanical properties, it is used in all sectors of industry, offerin.. |