Polymer Property : Charpy Impact, Notched = 10.1 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.26 - 2.12 J/cm²
6.00 - 10.1 ft-lb/in²
Average value: 1.61 J/cm² Grade Count:3
Overview of materials for Cellulose Acetate Butyrate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value..