Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.310 - 0.370 J/cm² @Temperature -30.0 - -30.0 °C |
1.48 - 1.76 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.340 J/cm² Grade Count:2 |
Overview of materials for PETG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |