Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.72 J/cm² @Temperature 23.0 °C |
8.18 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1A |
Gromax BFG45-B100N1 Nylon 6 46% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact, Notched | 1.72 J/cm² @Temperature -30.0 °C |
8.19 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® AZM 50 NOIR T6LD Nylon 12, 50% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-090,GF50Rigid grade with glass fiber (50%) for injection molding. Available color: black. Reinforced light and heat stabilizing agent. Mold-release agent.High rigid.. |