Polymer Property : Charpy Impact, Notched = 1.66 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.66 J/cm²

@Temperature 23.0 °C
7.90 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1A
Gromax CFG33-RN13N1 Nylon 6 33% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.