Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.21 J/cm²

@Temperature 23.0 °C
5.76 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1A
Gromax BFG30-BN00N1 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Charpy Impact, Notched 1.21 J/cm²

@Temperature -30.0 °C
5.76 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® AZM 30 GT8LD Nylon 12, 30% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA12,MHLS,16-050,(G+C)(F+D)(30+05)Rigid grade with glass fiber (30%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab..
Charpy Impact, Notched 1.21 J/cm²
5.76 ft-lb/in²
Arkema Group Rilsan® BZM 43 G9 Nylon 11, 43% Glass Fiber Filled (Dry)
Designation ISO 1874-PA11,MS,18-080,(G+C)(F+D)(45+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Additive free.High rigidity. Hig..