Polymer Property : Charpy Impact, Notched = 1.200 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.200 J/cm²

@Temperature 23.0 °C
5.710 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/1eA
FKuR Kunststoff Bio-Flex® F 2201 CL Compostable PLA Blend
The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta..