Polymer Property : Charpy Impact, Notched = 1.18 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.247 J/cm²
1.18 ft-lb/in²
ASTM D256
Plenco 4304 Phenolic, Nodular, Transfer Molded
PLENCO 04304 is a heat resistant, mineral filled phenolic molding compound offering improved mechanical strength properties along with excellent dimensional stability. UL recognized under component ..