Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.13 J/cm² | 5.38 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® FR50 NC010A Nylon 66
(Unverified Data**) 25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR50 NC010A is a 25% glass fiber reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performanc.. |
|||
Charpy Impact, Notched | 1.13 J/cm² | 5.38 ft-lb/in² | |
Arkema Group Rilsan® AZM 15 TLD Nylon 12, 15% Glass Fiber Filled (Dry) Designation ISO 1874-PA12,MHLR,16-030,GF15Rigid grade with glass fiber filler (15%) for injection molding.Available color: natural. Light and heat stabilized. Mold-release agent.Rigidity combined wi.. |