Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.12 J/cm²
5.33 ft-lb/in²
ISO 179/1eA
NOVA Chemicals Dylark® 378P30 Glass Reinforced Engineering Resin
Features: Ultra high modulus, High heat resistance, excellent adhesion to urethaneApplications: Instrument panel substrates, Brackets, Structural components
Charpy Impact, Notched 1.12 J/cm²

@Temperature -30.0 °C
5.33 ft-lb/in²

@Temperature -22.0 °F
Ineos ABS Centrex® 833 ASA+AES Blend  (discontinued **)
Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Profile extrusionSheet extrusionThermoformi..
Charpy Impact, Notched 1.12 J/cm²
5.33 ft-lb/in²
EN ISO 179/1eA
Wolf Kunststoff ZEDEX® ZX-410V7T A4T Polymer Alloy, Fiber Reinforced, Friction Modified
Main Characteristics: Fiber-reinforced; Friction-modified; Very high stiffness (higher than that of fiber-reinforced PEEK); Very low thermal expansion coefficient; Low friction; High wear resistance..