Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.08 J/cm²

@Temperature 23.0 °C
5.14 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1A
Gromax BFG30-AH00B3 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Charpy Impact, Notched 1.08 J/cm²
5.14 ft-lb/in²
ISO 179/1eA
Polyplastics Duranex® 531HS Polybutylene Terephthalate (PBT), Hydrolysis resistant, Heat shock resistant, Heat Shock Resistant
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Charpy Impact, Notched 1.08 J/cm²

@Temperature -40.0 °C
5.14 ft-lb/in²

@Temperature -40.0 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® FR50 NC010A Nylon 66  (Unverified Data**)
25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR50 NC010A is a 25% glass fiber reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performanc..