Charpy Impact, Notched 1.03 J/cm²

@Temperature -30.0 °C
4.90 ft-lb/in²

@Temperature -22.0 °F
Eastman Tenite 180A-28(HT) Cellulose Acetate  (discontinued **)
28% Plasticized.ISO data as provided by the manufacturer, Eastman Chemical.
Charpy Impact, Notched 1.03 J/cm²

@Temperature -30.0 °C
4.90 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Orgalloy® LE 60THM Flexible Nylon Alloy (Conditioned)
LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents).higher in rigidity than LE 6000. For film, hollow vessel blow moldi..