Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.940 J/cm² - NB | 4.47 ft-lb/in² - NB | Average value: 6.67 J/cm² Grade Count:65 |
Overview of materials for Polyester Thermoplastic Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact, Notched | 0.940 - 0.990 J/cm² @Temperature -30.0 - -30.0 °C |
4.47 - 4.71 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.965 J/cm² Grade Count:2 |
Overview of materials for Nylon 11 with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are includ.. |
|||
Charpy Impact, Notched | 0.940 J/cm² @Temperature -30.0 °C |
4.47 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® BZM 23 G9 Nylon 11, 23% Glass Fiber Filled (Dry) Designation ISO 1874-PA11,MS,18-040,(G+C)(F+D)(25+05)Rigid grade with glass fiber (23%) and graphite filler for injection molding. Available color: steel black gray. Additive free.Rigidity. Low fric.. |
|||
Charpy Impact, Notched | 0.940 J/cm² @Temperature -30.0 °C |
4.47 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® ASR 30 Nylon 12, 30% Carbon Fiber Filled (Dry) Designation ISO 1874-PA12,M,16-120,CF30Rigid grade with carbon fiber filler (30%) for injection molding. Available color: black.Very high rigidity. High strength-to-weight ratio. Very low shrinkage:.. |