Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.193 J/cm²
0.919 ft-lb/in²
ASTM D256
Plenco 2535 Phenolic, Granular, Compression Molded
PLENCO 02535 is a general purpose, organic filled phenolic molding compound offering optimized cure characteristics and excellent electrical properties. Type ASTM 5948 CFG, and UL recognized under c..
Charpy Impact, Notched 0.193 J/cm²
0.919 ft-lb/in²
ASTM D256
Plenco 5118 Phenolic, Granular, Transfer Molded
PLENCO 05118 is a mineral and graphite filled phenolic molding compound, formulated for bearing seals. 05118 provides for a low coefficient of friction, abrasion resistance, minimal water absorptio..