Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.917 J/cm²
4.36 ft-lb/in²
EN ISO 179/1eA
Wolf Kunststoff ZEDEX® ZX-530 A5D Polymer Alloy
Main Characteristics: Low Creep; Low moisture absorption; Flame retardant; Low impurity ions; Good machinability; FDA compliant LABS; Extremely low outgassing; Less expensive than PEEK; Stress resis..