Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.890 J/cm² | 4.24 ft-lb/in² | ISO 179 |
GEHR Plastics PEEK-30GF Polyetheretherketone, 30% Glass Fiber Polyether etherketone can be used at very high temperatures and it shows a good mechanical strength, toughness, hardness, flexural strength, and torsional strength. PEEK exhibits excellent chemical .. |
|||
Charpy Impact, Notched | 0.890 J/cm² @Temperature -30.0 °C |
4.24 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® BESN P40 TL Nylon 11, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA11-P,EHL,22-003Flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.High flexibility. High impact strength. Very good chemical res.. |