Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.145 J/cm² | 0.690 ft-lb/in² | ASTM D256 |
Plenco 5350 Phenolic, Granular, Compression Molded PLENCO 05350 is a mineral and graphite filled phenolic molding compound, developed for seal applications. PLENCO 05350 offers excellent dimensional stability, lubricity, and low abrasion properties... |