Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.320 - 0.650 J/cm²

@Temperature -30.0 - -30.0 °C
1.52 - 3.09 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.443 J/cm² Grade Count:4
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar..
Charpy Impact, Notched 0.400 - 0.650 J/cm²
1.90 - 3.09 ft-lb/in²
Average value: 0.575 J/cm² Grade Count:4
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m..
Charpy Impact, Notched 0.650 - 0.650 J/cm²

@Temperature -30.0 - -30.0 °C
3.09 - 3.09 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.650 J/cm² Grade Count:1
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m..
Copyright © lookpolymers.com All Rights Reserved