Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.530 J/cm²
2.52 ft-lb/in²
ISO 179/1eA
Nilit FRIANYL A63 SG10 Nylon 6.6 for injection molding, 10% mineral filled
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 0.530 J/cm²
2.52 ft-lb/in²
ISO 179/1eA
Nilit FRIANYL A63 SG15 Nylon 6.6 for injection molding, 15% mineral filled
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 0.530 J/cm²
2.52 ft-lb/in²
Eastman Eastar GN101 PETG Copolyester  (discontinued **)
ISO data as provided by the manufacturer, Eastman Chemical
Charpy Impact, Notched 0.530 J/cm²
2.52 ft-lb/in²
ISO 179/1eA
Lucite International Elvakon® 4494 Low Gloss Acrylic Capstock
Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr..
Charpy Impact, Notched 0.530 J/cm²
2.52 ft-lb/in²
ISO 179/1eA
Polyplastics Tepcon M270 Acetal-copolymer (POM), High Fluidity, High Cycle
Information provided by PolyPlastics.
Charpy Impact, Notched 0.530 J/cm²
2.52 ft-lb/in²
GB-1043
Zhejiang Juner PA-A6-3 GF/MF Reinforced
Applications: Shell of Middle & Top Grade MCB, Pedestal & Shell of Low Voltage Electrical ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd.
Charpy Impact, Notched 0.530 J/cm²
2.52 ft-lb/in²
ISO 179/1eA
Polyplastics Duranex® 711SA Polybutylene Terephthalate (PBT), Low density, Low wear, GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Charpy Impact, Notched 0.530 J/cm²
2.52 ft-lb/in²
50%RH; ISO 179/1eA
DuPont Performance Polymers Zytel® FE3734 NC010 Nylon 612  (Unverified Data**)
Unreinforced Polyamide 612 Zytel FE3734 NC010 is an unreinforced lubricated polyamide 612 resin suitable for injection molding.Information provided by DuPont Performance Polymers
Charpy Impact, Notched 0.530 J/cm²
2.52 ft-lb/in²
ISO 179/1eA
Polyplastics Duracon® M270-44/M270S Acetal Co-polymer (POM), Standard, High flow, High cycle
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
Charpy Impact, Notched 0.530 - 0.600 J/cm²

@Temperature -40.0 - -30.0 °C
2.52 - 2.86 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 0.560 J/cm² Grade Count:3
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m..
Charpy Impact, Notched 0.530 J/cm²
2.52 ft-lb/in²
ISO 179/1eA
Polyplastics Duracon® M270-45 Acetal Co-polymer (POM), Weather resistance, High flow, High cycle
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
Charpy Impact, Notched 0.530 J/cm²
2.52 ft-lb/in²
ISO 179/1eA
Polyplastics Duracon® M270-48 Acetal Co-polymer (POM), Antistatic, High flow
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..