Charpy Impact, Notched 0.466 J/cm²

@Temperature -30.0 °C
2.22 ft-lb/in²

@Temperature -22.0 °F
ASTM D256 and UNI EN ISO 179:1998
CRP Technology Windform® XT Polyamide-Carbon Composite
WindForm™ XT Composite is a new generation material, in which the mechanical characteristics are excellent for Rapid Manufacturing. Black coloured compound polyamide and carbon based material with ..