Charpy Impact, Notched 0.0800 - 0.800 J/cm²

@Temperature -30.0 - -20.0 °C
0.381 - 3.81 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.478 J/cm² Grade Count:10
Overview of materials for Nylon 66, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..