Polymer Property : Charpy Impact, Notched = 0.310 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.182 - 0.310 J/cm²
0.866 - 1.48 ft-lb/in²
Average value: 0.218 J/cm² Grade Count:15
Overview of materials for Phenolic, Novolac, Mineral/Flock Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Flock Filled". Each property range of values reported is minimum and maximum ..