Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.211 J/cm² | 1.00 ft-lb/in² | ASTM D256 |
Plenco 4568 Phenolic, Granular, Compression Molded PLENCO 04568 is a heat resistant, mineral and flock filled, phenolic molding compound, formulated to provide thermal oxidation stability along with excellent dimensional stability. 04568 is availabl.. |