Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.179 J/cm²
0.852 ft-lb/in²
ASTM D256
Plenco 05118-T5 Phenolic, Granular, Compression Molded
PLENCO 05118-T5 is a mineral and graphite filled novolac phenolic molding compound with PTFE, formulated for bearing seals. 05118 provides for a low coefficient of friction, good wear resistance, ve..
Charpy Impact, Notched 0.179 J/cm²
0.852 ft-lb/in²
ASTM D256
Plenco 2000 Phenolic, Granular, Injection Molded
PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under compo..