Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 641 MPa @Temperature -59.0 °C |
93000 psi @Temperature -74.2 °F |
Dry |
Hexcel® HexPly® F593 Epoxy Resin, F3T584 Carbon Fabric Hexcel designation: F3T584-42"-F593; Fiber: Toray T-300/3kInformation provided by HexCel |