Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.0621 MPa @Strain 25.0 % |
9.00 psi @Strain 25.0 % |
Typical value, 0.2"/min. strain rate |
Rogers Corporation Poron® 4701-30-25 Urethane Foam, Very Soft Very soft, easily compressed for use where flexibility is a key requirement. Standard available thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi.. |