Polymer Property : Compressive Yield Strength = 81000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 558 MPa

@Temperature 82.2 °C
81000 psi

@Temperature 180 °F
0°, Wet, Fill Compression
Hexcel® HexPly® 8552 Epoxy Matrix, SGP196-PW Fiber
Information provided by HexCel