Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 710 MPa @Temperature 104 °C |
103000 psi @Temperature 220 °F |
0°, Dry, Fill Compression |
Hexcel® HexPly® 8552 Epoxy Matrix, SGP196-PW Fiber Information provided by HexCel |
|||
Compressive Yield Strength | 710 MPa @Temperature 23.0 °C |
103000 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® F650 Bismaleimide Resin with Graphite F3T584 fabric reinforcement Aging Data, (T300-3K, 8 H.S.); Laminate Physicals: 59.6% Fiber volume, 34.0% Resin content, 1.0% VoidsInformation provided by HexCel |